Chery Automobile is recalling 20,193 Omoda and Tiggo vehicles in South Africa because a welding flaw in the rear‑axle could let a wheel detach, according to a notice from the manufacturer.
What Went Wrong in the Factory
The problem traces back to the rear‑axle manufacturing process. Poor welds were identified in the axle assemblies of vehicles built between 6 June 2022 and 31 December 2023. In plain terms, the welds that hold the axle together may not be strong enough, and in extreme cases the joint can fail, causing the rear wheel to come off and the driver to lose control.
How Many Cars Are Affected
The recall covers the Tiggo 5x SUV and Omoda models—most likely the Omoda 5 and Tiggo 7 Pro that are sold in South Africa. All 20,193 units will be inspected and, if needed, have the rear axle replaced at no charge to owners.
Is This a New Issue?
South Africa is the latest market to see the defect. Earlier this year China’s State Administration for Market Regulation ordered a recall of 53,882 Omoda and Tiggo vehicles for the same rear‑axle weld problem. Malaysia also recalled about 9,500 Omoda 5 cars in 2024 and 2026 after a high‑profile wheel‑detachment incident in Johor Bahru.
Why It Matters to Drivers
For everyday owners, the practical upshot is simple: a faulty rear axle can lead to a sudden loss of vehicle control, especially at highway speeds. That’s why Chery is urging owners to bring their cars to an authorized dealer for a free inspection and, if necessary, a replacement axle.
Chery’s Broader Expansion
While the recall draws attention to quality control, Chery is simultaneously pushing into new markets. The company, the fifth‑largest automaker in China with 2.8 million vehicles sold in 2025, is preparing to launch in Canada in early 2027 and is already operating an ex‑Nissan plant in South Africa. Its “Global Family” strategy emphasizes long‑term customer relationships, but the recall underscores the importance of robust manufacturing standards as the brand expands.
Owners in South Africa will be notified directly by Chery, and the replacement program is slated to begin this week.
Sources
- Chery
- There Is One Chinese Automaker That Is Inching Closer to the U.S. Market
- Chery recalls about 54,000 vehicles in China after Malaysia axle-failure incidents
- Chery Says North America Is So Important It Could Build Cars In Canada – CarScoops
- From One-Time Transactions to Full-Lifecycle Engagement: How Chery Is Redefining Customer Relationships Through Its 'Global Family” Approach
- MEPs ask European Commission to investigate BYD over cyber risks
Photo: Zoerides (CC BY-SA 4.0)